Desmopan? 9392A
Thermoplastic Polyurethane Elastomer
Extrusion- and injection molding grade; very good hydrolysis and microbial resistance; good low-temperature flexibility; Application; Hoses, non-reinforced; Cable sheathings; Profiles; Technical parts
Features | - Hydrolysis Resistant,Low Temperature Flexibility,Microbe Resistant
|
Uses | - Engineering Parts,Hose,Profiles
|
Processing Method | - Extrusion,Injection Molding
|
Density (73°F) | 1.15 | g/cm3 | ISO 1183 |
Shore Hardness |
|
| ISO 7619 |
Shore A, 1 sec, 73°F | 92 |
|
|
Shore D, 1 sec, 73°F | 42 |
|
|
Tensile Stress 2 |
|
| DIN 53504 |
Break, 73°F | 7250 | psi |
|
100% Strain, 73°F | 1600 | psi |
|
300% Strain, 73°F | 4350 | psi |
|
Tensile Strain 2 (Break, 73°F) | 400 | % | DIN 53504 |
Abrasion Resistance 3 | 20.0 | mm3 | ISO 4649 |
Tensile Storage Modulus |
|
| ISO 6721 |
-4°F | 102 | ksi |
|
68°F | 19.1 | ksi |
|
140°F | 10.3 | ksi |
|
Torsional Storage Modulus |
|
| ISO 6721 |
-4°F | 15084 | psi |
|
73°F | 3191 | psi |
|
158°F | 1885 | psi |
|
Tear Strength 4 (73°F) | 490 | lbf/in | ISO 34-1 |
Compression Set |
|
| ISO 815 |
73°F, 72 hr | 20 | % |
|
158°F, 24 hr 3 | 55 | % |
|
158°F, 24 hr 5 | 37 | % |
|
Rebound Resilience | 32 | % | ISO 4662 |
Drying Temperature | < 176 | °F |
|
Processing (Melt) Temp | 410 to 446 | °F |
|
Mold Temperature | 68 to 104 | °F |
|
Drying Temperature | < 176 | °F |
|
Melt Temperature | 383 to 419 | °F |
|