Elastollan? C95A exhibits excellent abrasion resistance and toughness, good hydrolytic stability, good heat, oil, fuel and solvent resistance. It has excellent damping characteristics and outstanding resistance to tear propagation. Elastollan? C95A is supplied uncolored in diced or pelletized form.
Appearance | |
Processing Method | ExtrusionInjection Molding |
Density / Specific Gravity | 1.21 |
| ASTM D792 |
Melt Mass-Flow Rate (MFR) (215°C/21.6 kg) | 50 to 110 | g/10 min | ASTM D1238 |
Durometer Hardness (Shore A) | 95 |
| ASTM D2240 |
Tensile Modulus (Injection Molded) | 9000 | psi | ASTM D412 |
Flexural Modulus (Injection Molded) | 11000 | psi | ASTM D790 |
Taber Abrasion Resistance | 30.0 | mg | ASTM D1044 |
Abrasion - DIN | 25 | mm3 | DIN 53516 |
Tensile Stress |
|
| ASTM D412 |
100% Strain | 2200 | psi |
|
300% Strain | 5300 | psi |
|
Tensile Strength | 6700 | psi | ASTM D412 |
Tensile Elongation (Break) | 440 | % | ASTM D412 |
Tear Strength 2 | 870 | lbf/in | ASTM D624 |
Compression Set |
|
| ASTM D395B |
73°F, 22 hr | 30 | % |
|
158°F, 22 hr | 45 | % |
|
Glass Transition Temperature | -32.8 | °F | Internal Method |
Vicat Softening Temperature | 275 | °F | ASTM D1525 |
Softening Point - DMA | 253 | °F | Internal Method |
Drying Temperature | 230 to 248 | °F |
|
Drying Time | 2.0 to 3.0 | hr |
|
Suggested Max Moisture | 0.030 | % |
|
Rear Temperature | 374 to 428 | °F |
|
Middle Temperature | 374 to 428 | °F |
|
Front Temperature | 374 to 428 | °F |
|
Nozzle Temperature | 410 to 437 | °F |
|
Drying Temperature | 230 to 248 | °F |
|
Drying Time | 2.0 to 3.0 | hr |
|
Cylinder Zone 1 Temp. | 338 to 410 | °F |
|
Cylinder Zone 3 Temp. | 338 to 410 | °F |
|
Cylinder Zone 5 Temp. | 338 to 410 | °F |
|
Adapter Temperature | 392 to 428 | °F |
|
Die Temperature | 383 to 419 | °F |
|