Texin? 245
熱塑性聚氨酯彈性體(聚酯)
Texin 245 resin is an aromatic polyester-based thermoplastic polyurethane with a Shore hardness of approximately 43D. It can be processed by injection molding; extrusion processes are not recommended.
特性 | - 抗撞擊性良好、良好的柔韌性、良好耐磨損性、耐低溫、耐燃油性、耐油性能、韌性良好
|
用途 | |
機(jī)構(gòu)評(píng)級(jí) | - FDA 21 CFR 177.1680,F(xiàn)DA 21 CFR 177.2600
|
加工方法 | |
密度 / 比重 |
|
|
|
-- | 1.21 |
| ASTM D792 |
-- | 1.21 | g/cm3 | ISO 1183 |
收縮率 |
|
|
|
流動(dòng) : 0.100 in | 8.0E-3 | in/in | ASTM D955 |
橫向流動(dòng) : 0.100 in | 8.0E-3 | in/in | ASTM D955 |
橫向流量 : 0.100 in | 0.80 | % | ISO 2577 |
流量 : 0.100 in | 0.80 | % | ISO 2577 |
肖氏硬度 (邵氏 D) | 43 |
| ASTM D2240, ISO 868 |
彎曲模量 |
|
| ASTM D790, ISO 178 |
73°F | 9990 | psi |
|
158°F | 7500 | psi |
|
泰伯耐磨性 |
|
|
|
1000 Cycles, 1000 g, H-18 轉(zhuǎn)輪 | 70.0 | mg | ASTM D1044 |
1000 Cycles, 1000 g, H-18 轉(zhuǎn)輪 | 70.0 | mg | ISO 4649 |
拉伸應(yīng)力 |
|
| ASTM D412, ISO 37 |
50%應(yīng)變 | 1100 | psi |
|
100%應(yīng)變 | 1310 | psi |
|
300%應(yīng)變 | 3000 | psi |
|
抗張強(qiáng)度 (屈服) | 7900 | psi | ASTM D412, ISO 37 |
伸長(zhǎng)率 (斷裂) | 500 | % | ASTM D412, ISO 37 |
撕裂強(qiáng)度 |
|
|
|
-- 2 | 700 | lbf/in | ASTM D624 |
-- | 700 | lbf/in | ISO 34-1 |
壓縮永久變形 |
|
|
|
73°F, 22 hr | 18 | % | ASTM D395B, ISO 815, ISO 815 |
158°F, 22 hr | 43 | % | ASTM D395B, ISO 815 |
158°F, 22 hr 3 | 35 | % | ASTM D395B, ISO 815 |
212°F, 22 hr | 60 | % | ASTM D395B, ISO 815 |
212°F, 22 hr 3 | 35 | % | ASTM D395B, ISO 815 |
巴肖氏彈性 | 45 | % | ASTM D2632 |
懸壁梁缺口沖擊強(qiáng)度 |
|
| ASTM D256 |
-22°F, 0.125 in | 3.3 | ft·lb/in |
|
73°F, 0.125 in | 無(wú)斷裂 |
|
|