Akulon? S225-KS
聚酰胺66
產(chǎn)品說明:
Flame Retardant (halogen free), Heat Stabilized
Special Features:
Akulon? is our family of high performance polyamide 6 and polyamide 66 materials, used by customers across the world in applications ranging from automotive, electronics & electrical, to furniture and packaging.
We offer Akulon? grades for injection molding, blow molding and extrusion (including barrier film, stock shapes, convoluted tubes, and mono and multi filament).
In molded parts the material offers an excellent balance of easy design and processing with outstanding mechanical properties over a wide temperature range and in diverse conditions. Meanwhile for extrusion the strength, resilience and easy processing of Akulon? sets the market standards.
密度 | 1.16 | -- | g/cm3 | ISO 1183 |
吸水率 |
|
|
| ISO 62 |
飽和, 73°F | 7.5 | -- | % |
|
平衡, 73°F, 50% RH | 2.2 | -- | % |
|
拉伸模量 | 580000 | 247000 | psi | ISO 527-2 |
拉伸應(yīng)力 (屈服) | 12300 | 5800 | psi | ISO 527-2 |
拉伸應(yīng)變 (屈服) | 4.0 | 20 | % | ISO 527-2 |
標(biāo)稱拉伸斷裂應(yīng)變 | 12 | 50 | % | ISO 527-2 |
簡(jiǎn)支梁缺口沖擊強(qiáng)度 (73°F) | 1.7 | 3.3 | ft·lb/in2 | ISO 179/1eA |
簡(jiǎn)支梁無缺口沖擊強(qiáng)度 (73°F) | 無斷裂 | 無斷裂 |
| ISO 179/1eU |
熱變形溫度 |
|
|
|
|
66 psi, 未退火 | 419 | -- | °F | ISO 75-2/B |
264 psi, 未退火 | 194 | -- | °F | ISO 75-2/A |
熔融溫度 3 | 500 | -- | °F | ISO 11357-3 |
線形熱膨脹系數(shù) |
|
|
| ISO 11359-2 |
流動(dòng) | 3.9E-5 | -- | in/in/°F |
|
橫向 | 7.8E-5 | -- | in/in/°F |
|
體積電阻率 | 1.0E+15 | 1.0E+13 | ohms·cm | IEC 60093 |
介電強(qiáng)度 | 760 | 640 | V/mil | IEC 60243-1 |
相對(duì)電容率 |
|
|
| IEC 60250 |
100 Hz | 2.80 | 7.00 |
|
|
1 MHz | 3.30 | 3.80 |
|
|
耗散因數(shù) |
|
|
| IEC 60250 |
100 Hz | 8.5E-3 | 0.14 |
|
|
1 MHz | 0.012 | 0.090 |
|
|
漏電起痕指數(shù) | 600 | 600 | V | IEC 60112 |
可燃性等級(jí) |
|
|
| IEC 60695-11-10, -20 |
0.015 in | V-0 | -- |
|
|
0.030 in | V-0 | -- |
|
|
0.06 in | V-0 | -- |
|
|
極限氧指數(shù) | 36 | -- | % | ISO 4589-2 |
熔體導(dǎo)熱性 | 0.90 | -- | Btu·in/hr/ft2/°F |
|
Specific Heat Capacity of Melt | 0.657 | -- | Btu/lb/°F |
|
干燥溫度 | 176 | °F |
|
干燥時(shí)間 | 4.0 到 8.0 | hr |
|
料筒后部溫度 | 482 到 500 | °F |
|
料筒中部溫度 | 500 到 518 | °F |
|
料筒前部溫度 | 509 到 527 | °F |
|
射嘴溫度 | 500 到 509 | °F |
|
加工(熔體)溫度 | 509 到 527 | °F |
|
模具溫度 | 122 到 176 | °F |
|
注射速度 | 中等偏快 |
|
|
背壓 | 435 到 1450 | psi |
|
螺桿壓縮比 | 2.5:1.0 |
|
|
如需恩驊力(Envalior)原廠物性表及相關(guān)文件,請(qǐng)聯(lián)系我司工作人員,謝謝!