熱塑性聚氨酯彈性體(聚酯)
產(chǎn)品說明:
Elastollan? C59D exhibits excellent abrasion resistance and toughness, good hydrolytic stability, good heat, oil, fuel and solvent resistance. It has excellent damping characteristics and outstanding resistance to tear propagation. Elastollan? C59D is rated UL-94 V-2 in vertical flame test for wall thickness of 0.75 mm. Elastollan? C59D is supplied uncolored in diced form.
密度 / 比重 | 1.23 |
| ASTM D792 |
肖氏硬度 (邵氏 D) | 56 |
| ASTM D2240 |
拉伸模量 (注塑) | 19000 | psi | ASTM D412 |
彎曲模量 (注塑) | 20000 | psi | ASTM D790 |
泰伯耐磨性 | 45.0 | mg | ASTM D1044 |
Abrasion - DIN | 25 | mm3 | DIN 53516 |
拉伸應(yīng)力 |
|
| ASTM D412 |
100%應(yīng)變 | 3400 | psi |
|
300%應(yīng)變 | 6700 | psi |
|
抗張強(qiáng)度 | 7300 | psi | ASTM D412 |
伸長率 (斷裂) | 430 | % | ASTM D412 |
撕裂強(qiáng)度 2 | 1200 | lbf/in | ASTM D624 |
壓縮永久變形 |
|
| ASTM D395B |
73°F, 22 hr | 30 | % |
|
158°F, 22 hr | 50 | % |
|
玻璃轉(zhuǎn)化溫度 | 5.00 | °F | 內(nèi)部方法 |
維卡軟化溫度 | 289 | °F | ASTM D1525 |
Softening Point - DMA | 268 | °F | 內(nèi)部方法 |
UL 阻燃等級 (0.030 in) | V-2 |
| UL 94 |
干燥溫度 | 230 到 248 | °F |
|
干燥時(shí)間 | 2.0 到 3.0 | hr |
|
建議的最大水分含量 | 0.030 | % |
|
料筒后部溫度 | 410 到 446 | °F |
|
料筒中部溫度 | 410 到 446 | °F |
|
料筒前部溫度 | 410 到 446 | °F |
|
射嘴溫度 | 428 到 464 | °F |
|